1. What is an Incoloy 800(N08800) sheet/plate?
The alloy plate made of Incoloy 800 (N08800) has high strength, high temperature, and high corrosion resistance. Nickel, iron, chromium, and titanium are some of its primary constituents. It is a superb material, especially ideal for usage in high temperature, high pressure, and extremely corrosive situations due to the proportions and properties of these components.
Excellent corrosion resistance and resistance to erosion by various acids, alkalis, salts, and other chemical compounds are both characteristics of the Incoloy 800 (N08800) alloy plate. It can maintain good stability without corrosion, deformation, or other issues in extreme settings, such as high temperature, high pressure, and strong acid and alkali conditions, and this can significantly increase its service life.
Incoloy 800(N08800) alloy plate has good high-temperature performance. It can work stably for a long time at temperatures up to 1100°C without problems such as embrittlement and deformation. In addition, the Incoloy 800 Incoloy alloy plate has excellent mechanical properties. Its high strength and excellent toughness enable it to withstand a large amount of mechanical stress without problems such as breakage. This also makes it ideal for manufacturing high-quality, high-reliability mechanical components.
2. Chemical composition of Incoloy 800 sheet/plate
Nickel (Ni): 30% ~ 35% Iron (Fe): 39.5% ~ 46% Chromium (Cr): 19% ~ 23% Copper (Cu): ≤0.75% Aluminum (Al): ≤0.15% Titanium (Ti): ≤0.15%
Steel Grade | Incoloy 800 | Incoloy 800H/800HT | Incoloy 825 | Incoloy 925 | Incoloy 926 |
Corresponding Brand | N08800/1.4876/ OCr20Ni32AITi / NS111 | N08810 / 1.4958 / NS112 | N08825 / 2.4858 / 0Cr21Ni42Mo3Cui2/ TNS142 | N09925 | N08926 / 1.4529 / Mo6CuN |
Chemical Composition | |||||
C⩽ | 0.100 | 0.05-0.1 | 0.050 | 0.030 | 0.020 |
Mn⩽ | 1.50 | 1.50 | 1.00 | 1.00 | 2.00 |
P⩽ | 0.030 | 0.030 | 0.030 | 0.030 | |
S⩽ | 0.015 | 0.015 | 0.030 | 0.030 | 0.010 |
Si⩽ | 1.00 | 1.00 | 0.50 | 0.50 | 0.50 |
Cr⩽ | 19.0-23.0 | 19.0-23.0 | 19.5-23.5 | 19.5-22.5 | 19.0-21.0 |
Ni⩽ | 30.0-35.0 | 30.0-35.0 | 38.0-46.0 | 42.0-46.0 | 24.0-26.0 |
Mo | 2.5-3.5 | 2.5-3.5 | 6.0-7.0 | ||
Cu | ≤0.75 | ≤0.75 | 1.50-3.0 | 1.50-3.0 | 0.50-1.0 |
N | 0.15-0.25 | ||||
Nb | 0.50 | ||||
other | AI:0.15-0.60 Tr:0.15-0.60 | AI:0.15-0.60 Tr:0.15-0.60 | AI:≤0.20 Tr:0.60-1.20 | Tr:1.9-2.4 AI:0.1-0.5 |
3. Mechanical properties of Incoloy 800 sheet/plate
1. Strength: Incoloy 800 has high strength, especially at high temperatures. Its yield strength can reach about 240 MPa at room temperature and about 140 MPa at high temperature (about 650°C).
2. Ductility: Incoloy 800 has good ductility and can maintain a certain plastic deformation ability at high temperatures. Its elongation at break is typically 30% or higher at room temperature while maintaining high ductility at high temperatures.
3. Hardness: Incoloy 800 has moderate hardness and provides good scratch and wear resistance. Its hardness is typically 120 to 140 HB at room temperature.
4. Creep performance: Incoloy 800 has good creep resistance at high temperatures and can withstand creep deformation when exposed to high temperatures and high-stress environments for a long time. It generally has a longer creep life and higher creep strength.
5. High-temperature stability: Incoloy 800 maintains good mechanical properties and corrosion resistance in high-temperature environments, and the maximum operating temperature can reach 1100°C.
6. Good corrosion resistance: Incoloy 800 has good corrosion resistance in corrosive environments such as strong acids and strong alkalis.
7. Magnetic properties: Incoloy 800 has low magnetic permeability and is suitable for situations where non-magnetic materials are required.
8. Dimensional stability: Incoloy 800 can maintain dimensional stability at high temperatures and is not prone to deformation and breakage.
Heat treatment or condition | Tensile strength σb ksi | Yield point σs ksi | Elongation or elongation after break δ % | Rate of reduction in area ψ % | Shock absorbs energy KV2 J |
---|---|---|---|---|---|
Annealing | ≥87 | ≥47 | ≥42 | ≥69 | ≥280 |
4. Physical properties of Incoloy 800 sheet/plate
Density: 7.95 g/cm³ Melting point: 1357-1385°C Thermal conductivity: 11.5 W/(m·K) (room temperature) Linear expansion coefficient: 14.7 μm/m°C (20-100°C)
Property | Imperial | Metric |
---|---|---|
Specific Heat, Btu/lb•°F (J/kg•°C). | 0.11 | 460 |
Curie Temperature, °F (°C). | -175 | -115 |
Permeability at 200 Oersted (15.9 kA/m) | 1.014 | |
Coefficient of Expansion, 10-6 in/in•°F (µm/m•°C) 70-200°F (20-100°C) | 7.9 | 14.4 |
5. Specifications of Incoloy 800 sheet/plate
Being a trustworthy Incoloy 800 sheet/plate manufacturer and supplier, Shanghai Yinggui Metal Pbaructs Company aims to make manufacturing easier for our business partners. Shanghai Yinggui Metal offers Incoloy 800, 825, 900, 901, 925, 926 etc.
item | value |
Product name | Inconel 625, 800, 825, 901, 925, 926 sheet |
Place of Origin | Shanghai China |
Type | Nickel alloy plate |
Application | Industry |
Grade | Nickel |
Ni (Min) | 60% |
Resistance (μΩ.m) | NA |
Powder Or Not | Not Powder |
Ultimate Strength (≥ MPa) | 830 |
Elongation (≥ %) | 30 |
Model Number | Inconel alloy |
Shape | wire |
Material | Nickle Alloy Material |
Surface | Bright |
Thickness | customized |
Certificate | CE ISO |
DELIVERY TIME | 7-15 Working Days |
Technique | Cold Rolled Hot Rolled |
Payment terms | L/C T/T (30% Deposit) |
MOQ | 10kg |
6. Applications and characteristics of Incoloy 800 sheet/plate
Performance characteristics of Incoloy 800 sheet/plate steel
Due to its many distinctive qualities, in high-temperature situations, Incoloy 800 is frequently employed. First of all, it has great oxidation resistance and can function steadily for a long time at high temperatures. Second, it has exceptional corrosion resistance and can withstand both alkaline and acidic media erosion. The substance also exhibits strong resistance to hydrogen embrittlement and stress corrosion cracking.
Many corrosive media are resistant to Incoloy 800. Due to its high nickel concentration, it resists stress corrosion cracking in harsh aqueous environments quite well. It is more resistant to pitting and crevice corrosion cracking due to the high chromium content. Although this alloy has low corrosion resistance to sulfuric and hydrochloric acids, it has considerable corrosion resistance to nitric and organic acids. It has strong corrosion resistance in oxidizing and non-oxidizing salts in addition to the potential for pitting corrosion in halides. Additionally, it has good corrosion resistance in water, steam, and steam, air, and carbon dioxide mixes.
Retort furnaces, heaters, stills, bubble columns, and condensers in fatty acid processes, evaporator tubes, tube sheets, and tableting trays in titanium dioxide plants, nuclear generators, nitric acid coolers, acetic anhydride cracking tubes, heat exchange equipment, heat exchange tubes, retort furnaces, muffle furnaces, and heat treatment fixtures and baskets, vacuum furnace devices
Incoloy 800 Application Areas
Incoloy 800 is widely used in various fields under high-temperature environments. It is often used in stoves, petrochemical equipment, chemical equipment, nuclear power plants, heat treatment furnaces, oil refining equipment, and the power industry. In addition, it is used to manufacture high-temperature equipment such as furnace tubes, heat exchangers, heaters, storage tanks, and pipes.
7. Main nickel-based alloy product brand list
Name | China GB | U.S.A UNS | Germany SEW VDIUV | U.K. BS | France AFNOR |
Incoloy 800 | NS111 | N08800 | W.Nr.1.4876 X10NiCrAlTi3220 | NA15 | Z8NC32.21 |
Incoloy 800H | NS112 | NO8810 | W.Nr.1.4958 X5 NiCrAlTi 31-20 | NA 15 (H) | |
Incoloy 800HT | N08811 | W.Nr.1.4959* X 8 NiCrAlTi 32-21 | |||
Incoloy 825 | NS142 | N08825 | W.Nr.2.4858 NiCr21Mo | NA16 | NC21FeDu |
Incoloy 800 | NS312 | N06800 | W.Nr.2.4816 NiCrl 5Fe | NA14 | NC15FE |
Incoloy 601 | NS313 | N06601 | W.Nr.2.4851 NiCr23Fe | NC23FeA | |
Incoloy 625 | NS336 | N06625 | W.Nr.2.4856 NiCr22Mo9Nb | NA21 | NC 22 DNb |
Incoloy 718 | GH4169 | N07718 | W.Nr.2.4668 NiCr19Fe19Nb5Mo3 | NA 51 | NC19FeNb |
Incoloy 926 | N08926 | W.Nr.1.4529 X1NiCrMoCu | X1NiCrMoCu | X1NiCrMoCu | |
Incoloy X-750 | GH4145 | N07750 | W.Nr.2.4669 NiCr15Fe7TiAl | NC15TNbA | |
Monel 400 | N04400 | W.Nr.2.4360 NiCu30Fe | NA 12 | Nu 30 | |
Hastelloy B | Ns321 | N10001 | |||
Hastelloy B-2 | NS322 | N10665 | W.Nr.2.4617 NiMo28 | NiMo28 | |
Hastelloy C | NS333 | ||||
Hastelloy C-22 | N06022 | W.Nr.2.4602 | |||
Hastelloy C276 | NS334 | N10276 | W.Nr.2.4819 NiMo16Cr15W | NC17D | |
254SMO | S31254 | W.Nr.1.4547 | |||
904L | N08904 | W.Nr.1.4539 | |||
GH1140 | GH1140 | ||||
GH2132 | GH2132 | S66286 | W.Nr.1.4890 | ||
GH3030 | GH3030 | ||||
GH3044 | GH3044 | ||||
GH3128 | GH3128 | ||||
Carpenter 20 | NS143 | N08020 | W.Nr.2.4660 NiCr20CuMo | ||
Alloy31 | N08031 | W.Nr.1.4562 X1NiCrMoCu32-28-7 | |||