1. What is a Monel 400(N04400) pipe/tube?
Solid solution alloy Monel 400 can only be cold-worked to harden it. This nickel alloy provides a high strength, superior weldability, and corrosion resistance. It is frequently employed in marine applications and other non-oxidizing chloride solutions due to its low corrosion rates in fast-flowing brackish or seawater, high resistance to stress corrosion cracking in most freshwaters, and resistance to a wide range of corrosive environments.
2. Chemical composition of Monel 400(N04400) pipe/tube
Monel400 alloy's primary chemical components are 30% Cu and 65% Ni, with a trace quantity of Fe (1%–2%) being present. A typical single-phase austenite structure describes the organizational structure. There is typically no intermetallic phase precipitation since nickel and copper are soluble in any ratio.
It is possible to discern that the austenite matrix of this alloy contains very dispersed non-metallic inclusions, such as sulfides and silicates, under non-etching conditions using a metallographic microscope. Additionally, the existence of carbides may be seen under specific circumstances. It can come in a range of alloy grades due to variations in chemical makeup, although there aren't any really noticeable distinctions in how well they resist corrosion. In comparison to pure nickel and pure copper, the monel400 alloy is more resistant to corrosion when exposed to reducing and oxidizing environments, respectively.
Element | Content (%) |
---|---|
Nickel, Ni | Remainder |
Copper, Cu | 28-34 |
Iron, Fe | 2.5 max |
Manganese, Mn | 2 max |
Silicon, Si | 0.5 max |
Carbon, C | 0.3 max |
Sulphur, S | 0.024 |
3. Mechanical properties of Monel 400(N04400) pipe/tube
Excellent mechanical qualities are also present in the alloy Monel 400 at high temperatures. The yield strength and tensile strength of the Monel 400 alloy rise at high temperatures, but the elongation falls in tandem. For instance, the yield strength, tensile strength, and elongation of the alloy Monel 400 at 600 °C are 130 MPa, 370 MPa, and 25%, respectively.
Condition | Heat treatment or condition | Tensile strength σb Mpa | Yield point σs Mpa | Elongation or elongation after break δ % | Hardness HBW |
---|---|---|---|---|---|
pipe/tube | Annealing | 517~620 | 172 | 35~60 | 110~149 |
pipe/tube | Hot-Finished(except Hexagons over 2 1/8 inches and Angles) | 552~758 | 276~690 | 30~60 | 140~241 |
pipe/tube | Hot-Finished Hexagons over 2 1/8 inches and Angles | 517~690 | 207~379 | 30~50 | 130~184 |
pipe/tube | Cold drawing, stress relief | 579~827 | 379~690 | 22~40 | 160~225 |
Sheet/Plate | Hot-Rolled, As-Rolled | 517~655 | 276~517 | 45~30 | 125~215 |
Sheet/Plate | Hot rolled | 482~586 | 193~345 | 50~35 | 110~140 |
Sheet | Annealing | 482~586 | 207~310 | 45~35 | HRB 65~80 |
Sheet | Cold work, hardening | 690~827 | 621~758 | 15~2 | HRB ≥93 |
Cold rolled strip | Annealing | 482~586 | 172~310 | 55~35 | HRB ≤68 |
Cold rolled strip | Spring Temper | 690~965 | 621~896 | 15~2 | HRB ≥98 |
Seamless pipe | Cold drawn, Annealing | 482~586 | 172~310 | 50~35 | ≤75 |
Seamless pipe | Cold drawn, stress relief | 586~827 | 379~690 | 35~15 | HRB 85~100 |
Seamless pipe | Heat-Exchanger, Annealed | 482~586 | 193~310 | 50~35 | HRB ≤85 |
Seamless pipe | Heat-Exchanger, Stress-Relieved | 586~724 | 379~621 | 35~15 | HRB 85~97 |
Seamless pipe | Hot extrusion | Actual measurement | Actual measurement | Actual measurement | Actual measurement |
Seamless pipe | Tempering1(Annealing) | ≤586 | 207~310 | 45~30 | HRB ≤73 |
Seamless pipe | Tempering2(1/2-Hard) | 586~724 | 379~552 | 30~10 | HRB 75~97 |
Seamless pipe | Tempering3(Hard) | 758~896 | 621~758 | 10~3 | HRC 95~27 |
Cold drawn wire | Annealing | 482~655 | 207~379 | 45~25 | |
Cold drawn wire | Tempering1 | 586~690 | 345~517 | 30~20 | |
Cold drawn wire | 1/4-Hard | 655~827 | 448~655 | 25~15 | |
Cold drawn wire | 1/2-Hard | 758~931 | 586~827 | 15~8 | |
Cold drawn wire | 3/4-Hard | 862~1034 | 690~931 | 8~5 | |
Cold drawn wire | Full-Hard--Spring Temper | 1000~1241 | 862~1172 | 5~2 |
4. Physical properties of Monel 400(N04400) pipe/tube
1. Monel 400 (N04400) Monel alloy tensile strength: σb≥450Mpa. 2. Monel 400 (N04400) Monel alloy yield strength: σb≥170Mpa. 3. Monel 400 (N04400) Monel alloy elongation: δ≥30%.
Physical Properties | ||
Grade | Density | Melting Point |
Monel 400 | 8.83 g/cm3 | 1300℃-1390℃ |
5. Specifications of Monel 400(N04400) pipe/tube
Being a trustworthy Monel pipe/tube manufacturer and supplier, Shanghai Yinggui Metal Pbaructs Company aims to make manufacturing easier for our business partners. Shanghai Yinggui Metal offers Monel 400, 404, K500, R405 etc.
Product Name | Nickel Alloy Steel Pipe |
Standard | GB,AISI,ASTM,DIN,EN,JIS |
Grade | Monel 400 / Monel K-500 Inconel 600 / Inconel 601 / Inconel 625 / Inconel 617 / Inconel 690 / Inconel 718 / Inconel X-750 Incoloy A-286 / Incoloy 800 / Incoloy 800H / Incoloy 800HT Incoloy 825 / Incoloy 901 / Incoloy 925 / Incoloy 926 Hastelloy B / Hastelloy B-2 / Hastelloy B-3 / Hastelloy C / Hastelloy C-276 / Hastelloy C-22 Hastelloy C-4 / Hastelloy C-2000 / Hastelloy G-35 / Hastelloy X / Hastelloy N |
Inspection | TUV, SGS, BV, ABS, LR and so on |
Application | Chemical, Pharmaceutical & Bio-Medical, Petrochemical & Refinery, Environmental, Food Processing, Aviation, Chemical Fertilizer, Sewage Disposal, Desalination, Waste Incineration etc. |
Specification | Wire: 0.01-10mm Strip: 0.05*5.0-5.0*250mm Bar: φ4-50mm; Length 2000-5000mm Pipe: φ6-273mm;δ1-30mm;Length 1000-8000mm Sheet: δ 0.8-36mm; Width 650-2000mm; Length 800-4500mm |
6. Applications and characteristics of Monel 400(N04400) pipe/tube
Performance characteristics of Monel 400(N04400) pipe/tube steel
In environments including seawater, hydrochloric acid, nitric acid, phosphoric acid, and hydrofluoric acid, the Monel 400 alloy exhibits good corrosion resistance. Additionally, it has strong abrasion resistance and is a material that is frequently utilized in the industries of maritime engineering, chemical industry, aerospace, and pharmaceuticals.
Monel 400 application areas
1. Seamless water pipes and steam pipes in power plants 2. Seawater exchanger and evaporator 3. Sulfuric acid and hydrochloric acid environment 4. Crude oil distillation 5. Pump shafts and propellers for equipment used in seawater 6. The nuclear industry is used to manufacture equipment for uranium refining and isotope separation. 7. Manufacturing pumps and valves used in hydrochloric acid production equipment
Monel400 machining and welding
Monel400 is easy to form by hot processing, the temperature is within 927~1177, and slight deformation is enough at 649 degrees. Monel400 alloy is very easy to form. The heat treatment temperature is generally 871~982 degrees, but for the sake of performance and fine grains, the solid solution temperature should not be too high. Solid solution annealing is generally chosen between 871 and 982. Monel400 alloy has good welding performance. Different welding methods require different welding wires. Generally, Monel60 and 190 welding wires are selected.
7. Main nickel-based alloy product brand list
Name | China GB | U.S.A UNS | Germany SEW VDIUV | U.K. BS | France AFNOR |
Monel 400(N04400) | NS111 | N08800 | W.Nr.1.4876 X10NiCrAlTi3220 | NA15 | Z8NC32.21 |
Monel 400(N04400)H | NS112 | NO8810 | W.Nr.1.4958 X5 NiCrAlTi 31-20 | NA 15 (H) | |
Monel 400(N04400)HT | N08811 | W.Nr.1.4959* X 8 NiCrAlTi 32-21 | |||
Incoloy 825 | NS142 | N08825 | W.Nr.2.4858 NiCr21Mo | NA16 | NC21FeDu |
Monel 400(N04400) | NS312 | N06800 | W.Nr.2.4816 NiCrl 5Fe | NA14 | NC15FE |
Incoloy 601 | NS313 | N06601 | W.Nr.2.4851 NiCr23Fe | NC23FeA | |
Incoloy 625 | NS336 | N06625 | W.Nr.2.4856 NiCr22Mo9Nb | NA21 | NC 22 DNb |
Incoloy 718 | GH4169 | N07718 | W.Nr.2.4668 NiCr19Fe19Nb5Mo3 | NA 51 | NC19FeNb |
Incoloy 926 | N08926 | W.Nr.1.4529 X1NiCrMoCu | X1NiCrMoCu | X1NiCrMoCu | |
Incoloy X-750 | GH4145 | N07750 | W.Nr.2.4669 NiCr15Fe7TiAl | NC15TNbA | |
Monel 400 | N04400 | W.Nr.2.4360 NiCu30Fe | NA 12 | Nu 30 | |
Hastelloy B | Ns321 | N10001 | |||
Hastelloy B-2 | NS322 | N10665 | W.Nr.2.4617 NiMo28 | NiMo28 | |
Hastelloy C | NS333 | ||||
Hastelloy C-22 | N06022 | W.Nr.2.4602 | |||
Hastelloy C276 | NS334 | N10276 | W.Nr.2.4819 NiMo16Cr15W | NC17D | |
254SMO | S31254 | W.Nr.1.4547 | |||
904L | N08904 | W.Nr.1.4539 | |||
GH1140 | GH1140 | ||||
GH2132 | GH2132 | S66286 | W.Nr.1.4890 | ||
GH3030 | GH3030 | ||||
GH3044 | GH3044 | ||||
GH3128 | GH3128 | ||||
Carpenter 20 | NS143 | N08020 | W.Nr.2.4660 NiCr20CuMo | ||
Alloy31 | N08031 | W.Nr.1.4562 X1NiCrMoCu32-28-7 | |||
Invar 36 | K93800 | W.Nr.1.3912 Ni36 | X1NiCrMoCu | Fe-Ni36 |